IEC TR 62662:2010
Current
The latest, up-to-date edition.
Guidance for production, testing and diagnostics of polymer insulators with respect to brittle fracture of core materials
Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users
English
30-08-2010
FOREWORD
INTRODUCTION
1 Scope
2 Normative references
3 Terms and definitions
4 Description of brittle fracture
5 Identification of brittle fracture
6 Failure mechanisms
7 Risk assessment
8 Guidance for material selection and production
9 Preventive methods
Bibliography
IEC/TR 62662:2010(E) presents an analysis of the risk of influencing factors for brittle fracture of composite insulators that are mostly loaded in the tensile mode (suspension and tension insulators). Guidance is given to reduce the risk of in-service brittle fractures.
| Committee |
TC 36
|
| DevelopmentNote |
Stability Date: 2020. (09/2017)
|
| DocumentType |
Technical Report
|
| Pages |
17
|
| PublisherName |
International Electrotechnical Committee
|
| Status |
Current
|
| Standards | Relationship |
| IS 16686 : 2018 | Identical |
| NEN NPR IEC/TR 62662 : 2010 | Identical |
| CEI CLC/TR 62662 : 2012 | Identical |
| VDE 0674-278:2017-01 | Identical |
| S.R. CLC/TR 62662:2011 | Identical |
| DIN CLC/TR 62662:2017-01 | Identical |
| NEN NPR CLC IEC/TR 62662 : 2011 | Identical |
| BS PD IEC/TR 62662 : 2010 | Identical |
| CLC/TR 62662:2011 | Identical |
| UNE-CLC/TR 62662:2016 IN | Identical |
| UNE-CLC/TR 62662:2012 IN | Identical |