I.S. EN 50363-0:2011
Current
The latest, up-to-date edition.
INSULATING, SHEATHING AND COVERING MATERIALS FOR LOW-VOLTAGE ENERGY CABLES - PART 0: GENERAL INTRODUCTION
Hardcopy , PDF
English
01-01-2011
For Harmonized Standards, check the EU site to confirm that the Standard is cited in the Official Journal.
Only cited Standards give presumption of conformance to New Approach Directives/Regulations.
1 Scope
2 Normative references
3 Terms and definitions
4 Testing
5 Requirements
Bibliography
Specifies the requirements for insulating, sheathing and covering materials that are used for harmonized low voltage energy cables.
DocumentType |
Standard
|
Pages |
13
|
PublisherName |
National Standards Authority of Ireland
|
Status |
Current
|
Standards | Relationship |
SN EN 50363-0 : 2011 | Identical |
NBN EN 50363-0 : 2011 | Identical |
NF EN 50363-0 : 2012 | Identical |
EN 50363-0:2011 | Identical |
BS EN 50363-0:2011 | Identical |
DIN EN 50363-0 : 2012 | Identical |
NEN EN 50363-0 : 2011 | Identical |
UNE-EN 50363-0:2011 | Identical |
EN 50290-2-20:2016 | Communication cables - Part 2-20: Common design rules and construction - General |
IEC 60811-3-1:1985 | Common test methods for insulating and sheathing materials ofelectric cables - Part 3: Methods specific to PVC compounds -Section One: Pressure test at high temperature - Tests forresistance to cracking |
HD 622 S1:1996/A2:2005 | Power cables having rated voltages from 3,6/6 (7,2) kV up to and including 20,8/36 (42) kV with special fire performance for use in power stations |
HD 627 S1:1996/A2:2005 | MULTICORE AND MULTIPAIR CABLES FOR INSTALLATION ABOVE AND BELOW GROUND |
IEC 60684-2:2011 | Flexible insulating sleeving - Part 2: Methods of test |
EN 50267-2-1:1998 | Common test methods for cables under fire conditions - Tests on gases evolved during combustion of materials from cables - Part 2-1: Procedures - Determination of the amount of halogen acid gas |
IEC 60811-4-1:2004 | Insulating and sheathing materials of electric and optical cables - Common test methods - Part 4-1: Methods specific to polyethylene and polypropylene compounds - Resistance to environmental stress cracking - Measurement of the melt flow index - Carbon black and/or mineral filler content measurement in polyethylene by direct combustion - Measurement of carbon black content by thermogravimetric analysis (TGA) - Assessment of carbon black dispersion in polyethylene using a microscope |
EN 60684-2:2011 | Flexible insulating sleeving - Part 2: Methods of test |
EN 60811-3-2 : 95 AMD 2 2004 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC AND OPTICAL CABLES - COMMON TEST METHODS - PART 3-2: METHODS SPECIFIC TO PVC COMPOUNDS - LOSS OF MASS TEST - THERMAL STABILITY TEST |
EN 50290-2-27 : 2002 COR 2010 | COMMUNICATION CABLES - PART 2-27: COMMON DESIGN RULES AND CONSTRUCTION - HALOGEN FREE FLAME RETARDANT THERMOPLASTIC SHEATHING COMPOUNDS |
EN 60811-1-3:1995/A1:2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - PART 1-3: GENERAL APPLICATION - METHODS FOR DETERMINING THE DENSITY - WATER ABSORPTION TESTS - SHRINKAGE TEST |
HD 620 : 2010 | DISTRIBUTION CABLES WITH EXTRUDED INSULATION FOR RATED VOLTAGES FROM 3,6/6 (7,2) KV UP TO AND INCLUDING 20,8/36 (42) KV |
EN 50290-2-29:2016 | Communication cables - Part 2-29: Common design rules and construction - Crosslinked polyethylene insulation compounds: instrumentation, control and field bus cables |
HD 603 S1:1994/A3:2007 | DISTRIBUTION CABLES OF RATED VOLTAGE 0,6/1 KV |
EN 50290-2-23:2013 | COMMUNICATION CABLES - PART 2-23: COMMON DESIGN RULES AND CONSTRUCTION - POLYETHYLENE INSULATION FOR MULTI-PAIR CABLES USED IN ACCESS TELECOMMUNICATION NETWORKS: OUTDOOR CABLES |
PREN 50525-3-11 : DRAFT 2008 | ELECTRIC CABLES - LOW VOLTAGE ENERGY CABLES OF RATED VOLTAGES UP TO AND INCLUDING 450/750 V - PART 3-11: CABLES WITH SPECIAL FIRE PERFORMANCE - FLEXIBLE CABLES WITH HALOGEN-FREE THERMOPLASTIC INSULATION, AND LOW EMISSION OF SMOKE |
EN 50290-2-26 : 2002 AMD 1 2007 | COMMUNICATION CABLES - PART 2-26: COMMON DESIGN RULES AND CONSTRUCTION - HALOGEN FREE FLAME RETARDANT INSULATION COMPOUNDS |
EN 60811-3-1 : 95 AMD 2 2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - METHODS SPECIFIC TO PVC COMPOUNDS - PRESSURE TEST AT HIGH TEMPERATURE - TESTS FOR RESISTANCE TO CRACKING |
HD 626 S1:1996/A2:2002 | OVERHEAD DISTRIBUTION CABLES OF RATED VOLTAGE U[O]/U(U[M]): 0,6/1 (1,2) KV |
EN 50290-2-28:2002 | Communication cables - Part 2-28: Common design rules and construction - Filling compounds for filled cables |
IEC 60811-1-2:1985 | Common test methods for insulating and sheathing materials of electric cables - Part 1: Methods for general application - Section Two: Thermal ageing methods |
EN 60811-4-1:2004 | Insulating and sheathing materials of electric and optical cables - Common test methods - Part 4-1: Methods specific to polyethylene and polypropylene compounds - Resistance to environmental stress cracking - Measurement of the melt flow index - Carbon black and/or mineral filler content measurement in polyethylene by direct combustion - Measurement of carbon black content by thermogravimetric analysis (TGA) - Assessment of carbon black dispersion in polyethylene using a microscope |
EN 60811-1-2:1995/A2:2000 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - GENERAL APPLICATION - THERMAL AGEING METHODS |
IEC 60811-1-1:1993+AMD1:2001 CSV | Common test methods for insulating and sheathing materials of electric cables and optical cables - Part 1-1: Methods for general application - Measurement of thickness and overall dimensions - Tests for determining the mechanical properties |
EN 50290-2-30:2002 | Communication cables - Part 2-30: Common design rules and construction - Poly(tetrafluoroethylene-hexafluoropropylene) (FEP) insulation and sheathing |
EN 50395 : 2005 AMD 1 2011 | ELECTRICAL TEST METHODS FOR LOW VOLTAGE ENERGY CABLES |
EN 50290-2-25:2013 | COMMUNICATION CABLES - PART 2-25: COMMON DESIGN RULES AND CONSTRUCTION - POLYPROPYLENE INSULATION COMPOUNDS |
EN 60811-2-1 : 98 AMD 1 2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - PART 2-1: METHODS SPECIFIC TO ELASTOMERIC COMPOUNDS - OZONE RESISTANCE, HOT SET AND MINERAL OIL IMMERSION TESTS |
IEC 60811-1-3:1993+AMD1:2001 CSV | Common test methods for insulating and sheathing materials of electric and optical cables - Part 1-3: General application -Methods for determining the density - Water absorption tests - Shrinkage test |
EN 50290-2-22 : 2001 AMD 1 2007 | COMMUNICATION CABLES - PART 2-22: COMMON DESIGN RULES AND CONSTRUCTION - PVC SHEATHING COMPOUNDS |
IEC 60811-1-4:1985 | Common test methods for insulating and sheathing materials of electric cables - Part 1: Methods for general application - Section Four: Tests at low temperature |
IEC 60811-2-1:1998+AMD1:2001 CSV | Common test methods for insulating and sheathing materials of electric and optical cables - Part 2-1: Methods specific to elastomeric compounds - Ozone resistance, hot set and mineral oil immersion tests |
EN 50290-2-21:2001/A1:2007/AC:2016 | COMMUNICATION CABLES - PART 2-21: COMMON DESIGN RULES AND CONSTRUCTION - PVC INSULATING COMPOUNDS |
IEC 60811-3-2:1985 | Common test methods for insulating and sheathing materials of electric cables - Part 3: Methods specific to PVC compounds - Section Two: Loss of mass test - Thermal stability test |
EN 50267-2-2:1998 | Common test methods for cables under fire conditions - Tests on gases evolved during combustion of materials from cables - Part 2-2: Procedures - Determination of degree of acidity of gases for materials by measuring pH and conductivity |
EN 50290-2-24 : 2002 AMD 1 2008 | COMMUNICATION CABLES - PART 2-24: COMMON DESIGN RULES AND CONSTRUCTION - PE SHEATHING |
EN 50396 : 2005 AMD 1 2011 | NON ELECTRICAL TEST METHODS FOR LOW VOLTAGE ENERGY CABLES |
EN 60811-1-1:1995/A1:2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - GENERAL APPLICATION - MEASUREMENT OF THICKNESS AND OVERALL DIMENSIONS - TESTS FOR DETERMINING MECHANICAL PROPERTIES |
HD 604 S1:1994/A3:2005 | 0.6/1 KV POWER CABLES WITH SPECIAL FIRE PERFORMANCE FOR USE IN POWER STATIONS |
HD 621 S1:1996/A1:2001 | MV IMPREGNATED PAPER INSULATED DISTRIBUTION CABLES OF RATED VOLTAGES OF 3.8/6.6 KV TO 19/33 KV |
EN 60811-1-4:1995/A2:2001 | INSULATING AND SHEATHING MATERIALS OF ELECTRIC CABLES - COMMON TEST METHODS - PART 1-4: GENERAL APPLICATION - TESTS AT LOW TEMPERATURE |
Please Login or Create an Account so you can add users to your Multi user PDF Later.
Important note : All end users must be registered with an Account prior to user licenses being assigned.
Users cannot be edited or removed once added to your Multi user PDF.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.