BS 2L 97:1971
Withdrawn
Withdrawn
Specification for plate of aluminium-copper-magnesium-manganese alloy (solution treated, controlled stretched and aged at room temperature) (Cu 4.4, Mg 1.5, Mn 0.6)
Available format(s)
Hardcopy , PDF
Language(s)
English
Published date
08-31-1971
Publisher
Withdrawn date
09-24-2012
US$208.86
Excluding Tax where applicable
NO CONTENTS SECTION
Specifies plate made from aluminium and alloy constituents, with or without approved scrap, at the discretion of the manufacturer, including that which has been forged as an intermediate operation, which is finished by hot or cold rolling, but excludes forged plate.
| Committee |
ACE/61/-/24
|
| DevelopmentNote |
Supersedes 69/27775 DC, 91/73184 DC and BS L97(1968). (07/2005) Inactive for the new design. (12/2007)
|
| DocumentType |
Standard
|
| Pages |
8
|
| PublisherName |
British Standards Institution
|
| Status |
Withdrawn
|
| Supersedes |
| DEFSTAN 80-16/4(2006) : 2006 | PAINT REMOVER, DICHLOROMETHANE, WATER RINSABLE TYPE - TYPE 1: HIGH VISCOSITY (BRUSHING) TYPE 2: LOW VISCOSITY (SPRAYING) |
| DEFSTAN 05-133(PT1)/1(2011) : 2011 | METHODS FOR TESTING PAINTS, CHEMICALS AND ASSOCIATED PRODUCTS - PART 1: PAINTS AND ALLIED PRODUCTS |
| DEFSTAN 80-221/1(2009) : 2009 | PAINT REMOVER FOR AIR DRYING PAINT SCHEME FOR AEROSPACE PURPOSES - TYPE 1: HIGH VISCOSITY (BRUSHING) - TYPE 2: LOW VISCOSITY (SPRAYING) |
| DEFSTAN 80-16/3(2002) : 2002 | PAINT REMOVER, DICHLOROMETHANE, WATER RINSABLE - TYPE 1: HIGH VISCOSITY (BRUSHING) TYPE 2: LOW VISCOSITY (SPRAYING) |
| BS 2L 98:1971 | Specification for plate of aluminium-copper-magnesium-manganese alloy (solution treated and aged at room temperature: not controlled stretched) (Cu 4.4, Mg 1.5, Mn 0.6) |
| BS L 109:1971 | Specification for aluminium-coated sheet and strip of aluminium-copper-magnesium-manganese alloy (solution treated and aged at room temperature) (Cu 4.4, Mg 1.5, Mn 0.6) |
| BS L 110:1971 | Specification for aluminium-coated sheet and strip of aluminium-copper-magnesium-manganese alloy (supplied for solution treatment by the user) (Cu 4.4, Mg 1.5, Mn 0.6) |
| BS L 109:1971 | Specification for aluminium-coated sheet and strip of aluminium-copper-magnesium-manganese alloy (solution treated and aged at room temperature) (Cu 4.4, Mg 1.5, Mn 0.6) |
| BS L 110:1971 | Specification for aluminium-coated sheet and strip of aluminium-copper-magnesium-manganese alloy (supplied for solution treatment by the user) (Cu 4.4, Mg 1.5, Mn 0.6) |
| BS PD 5686(1969) : LATEST | THE USE OF SI UNITS |
| BS 3763:1970 | The International System of units (SI) |
| BS 350:2004 | Conversion factors for units |
| BS 2L 98:1971 | Specification for plate of aluminium-copper-magnesium-manganese alloy (solution treated and aged at room temperature: not controlled stretched) (Cu 4.4, Mg 1.5, Mn 0.6) |