BS EN 10025-6:2019
Withdrawn
Hot rolled products of structural steels Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition
Hardcopy , PDF
English
08-19-2019
04-12-2023
| Committee |
ISE/103
|
| DocumentType |
Standard
|
| ISBN |
978 0 580 73970 5
|
| Pages |
30
|
| ProductNote |
THIS STANDARD ALSO REFERS TO CR 10320
|
| PublisherName |
British Standards Institution
|
| Status |
Withdrawn
|
| Supersedes |
This document specifies technical delivery conditions for flat products of high yield strength alloy special steels. The grades and qualities are given in Tables 1 to 3 (chemical composition) and Tables 4 to 6 (mechanical properties) and are supplied in the quenched and tempered condition. The steels specified in this document are applicable to hot-rolled flat products with a minimum nominal thickness of 3 mm and a maximum nominal thickness of 200 mm for grades S460, S500, S550, S620 and S690, a maximum nominal thickness of 125 mm for grades S890 and S960, in steels which, after quenching and tempering, have a specified minimum yield strength of 460 MPa to 960 MPa.
| Standards | Relationship |
| EN 10025-6:2019 | Identical |
| I.S. EN 10025-6:2019 | Equivalent |
| DIN EN 10025-6:2019-10 | Equivalent |
| EN 10025-6:2019 | Equivalent |
| EN 10162:2003 | Cold rolled steel sections - Technical delivery conditions - Dimensional and cross-sectional tolerances |
| EN 10048:1996 | Hot rolled narrow steel strip - Tolerances on dimensions and shape |
| EN 10051:2010 | Continuously hot-rolled strip and plate/sheet cut from wide strip of non-alloy and alloy steels - Tolerances on dimensions and shape |
| EN 10027-2:2015 | Designation systems for steels - Part 2: Numerical system |
| EN 10029:2010 | Hot-rolled steel plates 3 mm thick or above - Tolerances on dimensions and shape |
| EN 10164:2004 | Steel products with improved deformation properties perpendicular to the surface of the product - Technical delivery conditions |
| EN ISO 1461:2009 | Hot dip galvanized coatings on fabricated iron and steel articles - Specifications and test methods (ISO 1461:2009) |
| ISO 1461:2009 | Hot dip galvanized coatings on fabricated iron and steel articles — Specifications and test methods |
| EN ISO 2566-1:1999 | Steel - Conversion of elongation values - Part 1: Carbon and low alloy steels (ISO 2566-1:1984) |
| EN 10025-1:2004 | Hot rolled products of structural steels - Part 1: General technical delivery conditions |
| EN 10163-2:2004 | Delivery requirements for surface condition of hot-rolled steel plates, wide flats and sections - Part 2: Plate and wide flats |
| ISO 14713:1999 | Protection against corrosion of iron and steel in structures — Zinc and aluminium coatings — Guidelines |
| ISO 2566-1:1984 | Steel — Conversion of elongation values — Part 1: Carbon and low alloy steels |
| EN 10027-1:2016 | Designation systems for steels - Part 1: Steel names |
| EN 10020:2000 | Definition and classification of grades of steel |
| CEN/TR 10347:2006 | Guidance for forming of structural steels in processing |
| EN 10160:1999 | Ultrasonic testing of steel flat product of thickness equal or greater than 6 mm (reflection method) |
| EN ISO 14713 : 1999 | PROTECTION AGAINST CORROSION OF IRON AND STEEL IN STRUCTURES - ZINC AND ALUMINIUM COATINGS - GUIDELINES |