DEFSTAN 93-83/1(1995) : 1995
Withdrawn
SYNTHETIC POLYISOPRENE RUBBER, BLACK TYPE MD, 40 IRHD
English
01-01-1995
09-12-2003
Preface
1 Scope
2 WARNING
3 Related documents
4 Composition
5 Ingredients
6 Processing conditions
7 Type approval
8 Test samples
9 Test requirements
10 Methods of test
11 Packaging
Table A
Annex A - Schedule for chemical tests
Gives requirements for a high quality black polyisoprene compound designated IR MD 40 intended for the manufacture of respirator components.
| DevelopmentNote |
Supersedes TS 50604 (07/2001)
|
| DocumentType |
Standard
|
| Pages |
14
|
| PublisherName |
UK Ministry of Defence Standards
|
| Status |
Withdrawn
|
| Supersedes |
| DEFSTAN 93-31/2(1983) : 1983 AMD 1 1984 | TEST PROCEDURES AND PROCESS REQUIREMENTS FOR FULLY COMPOUNDED UNVULCANIZED RUBBER |
| BS 903-A2:1989 | Physical testing of rubber Determination of tensile stress-strain properties |