DR 91014
Superseded
View Superseded by
Timber - Methods of test Method 1: Moisture content
02-15-2008
10-26-2017
Note - due to the age of this archived document, available information is limited therfore this record is incomplete. For further details, please phone our Customer Service Centre on 131 242 (Intl +61 2 8206 6010) or email sales@saiglobal.com.
Describes procedures for preparing specimens for test in the laboratory and in the field and is technically equivalent to the 1972 edition. This Standard describes two levels of precision, the primary and secondary method. It also incorporates temperature and species correction tables.
| CommentClosesDate |
03-31-1991
|
| Committee |
TM-003
|
| DocumentType |
Draft
|
| PublisherName |
Standards Australia
|
| Status |
Superseded
|
| SupersededBy |
Revision of AS 1080.1-1972