EN 1941 : 1996
Superseded
Superseded
View Superseded by
SELF ADHESIVE TAPES - MEASUREMENT OF ELONGATION AT BREAK
Published date
01-12-2013
Publisher
Superseded date
03-01-2003
Superseded by
Sorry this product is not available in your region.
Foreword
1 Scope
2 Definition
3 Principle
4 Apparatus
5 Test sample and test pieces
6 Procedure
7 Expression of results
8 Test report
Defines a method of measuring the elongation of a self adhesive tape subjected to tensile force sufficient for it to break. The maximum width of tape tested is 25 mm, but wider tape can be cut down to 25 mm with a sharp instrument.
| Committee |
TC 253
|
| DocumentType |
Standard
|
| PublisherName |
Comite Europeen de Normalisation
|
| Status |
Superseded
|
| SupersededBy |
| Standards | Relationship |
| NS EN 1941 : 1ED 1996 | Identical |
| NF EN 1941 : 1996 | Identical |
| BS EN 1941:1996 | Identical |
| I.S. EN 1941:1996 | Identical |
| NBN EN 1941 : 1996 | Identical |
| NEN EN 1941 : 1996 | Identical |
| UNE-EN 1941:1996 | Identical |
| DIN EN 1941:1996-04 | Identical |
| ASTM D 3759/D3759M : 2005 | Standard Test Method for Tensile Strength and Elongation of Pressure-Sensitive Tapes |
| ASTM D 3759/D3759M : 2005 : R2011 | Standard Test Method for Breaking Strength and Elongation of Pressure-Sensitive Tape |
| ASTM D 3022 : 1984 : R1996 : EDT 1 | Standard Test Method for Color and Strength of Color Pigments by Use of a Miniature Sandmill |
Summarise