NS EN 14187-9 : 1ED 2006
Withdrawn
View Superseded by
COLD APPLIED JOINT SEALANTS - TEST METHODS - PART 9: FUNCTION TESTING OF JOINT SEALANTS
01-12-2013
06-01-2019
Foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Principle
5 Apparatus and materials
5.1 Concrete test blocks
5.2 Tensile/compression test rig
5.3 Climate chamber
5.4 Temperature indicator
6 Preparation of the test specimens
7 Procedure
7.1 Conditioning cycle
7.2 After conditioning
7.3 Test procedure
8 Calculation and expression of results
9 Test report
Specifies a function test for cold applied joint sealants intended for use in joints in roads and airfield pavements in cold climate areas where the total joint movement can be greater than 35 % and the temperature can go below -25 degree C.
| DocumentType |
Standard
|
| PublisherName |
Norwegian Standards (Norges Standardiseringsforbund)
|
| Status |
Withdrawn
|
| SupersededBy |
| Standards | Relationship |
| EN 14187-9:2006 | Identical |
| NEN EN 14187-9 : 2006 | Identical |
| BS EN 14187-9:2006 | Identical |
| NBN EN 14187-9 : 2006 | Identical |
| DIN EN 14187-9:2006-05 | Identical |
| I.S. EN 14187-9:2006 | Identical |
| EN 14187-9:2019 | Identical |
| ONORM EN 14187-9 : 2006 | Identical |
| NF EN 14187-9 : 2006 | Identical |
| DIN EN 14187-9:2019-06 | Identical |
| UNE-EN 14187-9:2007 | Identical |