Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, Foil and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated

Available format(s)

Hardcopy , PDF

Language(s)

English

Published date

08-15-2016

Superseded date

11-19-2017

Superseded by

SAE AMS5596M

US$112.10
Excluding Tax where applicable

This specification covers a corrosion and heat-resistant nickel alloy in the form of sheet, strip, foil, and plate 1.00 inch (25.4 mm) and under in thickness (see8.5).

DocumentType
Standard
Pages
9
PublisherName
SAE International
Status
Superseded
SupersededBy
Supersedes

This specification covers a corrosion and heat-resistant nickel alloy in the form of sheet, strip, foil, and plate 1.00 inch (25.4 mm) and under in thickness (see 8.5).

SAE ARP699E High Temperature Pneumatic Duct Systems for Aircraft
ASTM F 3055 : 2014 Standard Specification for Additive Manufacturing Nickel Alloy (UNS N07718) with Powder Bed Fusion
ASTM F 3055 : 2014 : EDT 1 Standard Specification for Additive Manufacturing Nickel Alloy (UNS N07718) with Powder Bed Fusion
SAE AMS2774E Heat Treatment Wrought Nickel Alloy and Cobalt Alloy Parts

US$112.10
Excluding Tax where applicable