SAE MAM5536B
Withdrawn
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 47.5ni 22cr 1.5co 9.0mo 0.60w 18.5fe, Solution Heat Treated
Hardcopy , PDF
English
03-12-2003
03-12-2003
1. SCOPE
2. APPLICABLE DOCUMENTS
3. TECHNICAL REQUIREMENTS
4. QUALITY ASSURANCE PROVISIONS
5. PREPARATION FOR DELIVERY
6. ACKNOWLEDGMENT
7. REJECTIONS
8. NOTES
Includes corrosion and heat resistant nickel alloy in the form of sheet, strip, and plate procured in SI (metric) units. Used typically for parts requiring oxidation resistance up to 1205 degrees C and relatively high strength up to 815 degrees C.
| DocumentType |
Standard
|
| Pages |
7
|
| PublisherName |
SAE International
|
| Status |
Withdrawn
|
| Supersedes |
This specification covers a corrosion and heat resistant nickel alloy in the form of sheet, strip, and plate procured in SI (metric) units. AMS 5536 is the inch/pound version of this MAM. These products have been used typically for parts requiring oxidation resistance up to 1205 degrees C and relatively high strength up to 815 degrees C, but usage is not limited to such applications.
| SAE AMS 2269 : 2006 | CHEMICAL CHECK ANALYSIS LIMITS, NICKEL, NICKEL ALLOYS, AND COBALT ALLOYS |
| SAE MAM2262D | Tolerances, Metric, Nickel, Nickel Alloy, and Cobalt Alloy Sheet, Strip, and Plate |
| SAE AMS2371K | Quality Assurance Sampling and Testing Corrosion and Heat-Resistant Steels and Alloys Wrought Products and Forging Stock |
| ASTM E 8M : 2004 | Standard Test Methods for Tension Testing of Metallic Materials [Metric] (Withdrawn 2008) |
| MIL-STD-163 Revision C:1978 | Steel Mill Products Preparation for Shipment and Storage (S/S by ASTM-A700) |
| ASTM E 290 : 2014 : REDLINE | Standard Test Methods for Bend Testing of Material for Ductility |
| ASTM E 354 : 2014 : REDLINE | Standard Test Methods for Chemical Analysis of High-Temperature, Electrical, Magnetic, and Other Similar Iron, Nickel, and Cobalt Alloys |