TAPPI T 837 : 0
Withdrawn
MEASURING THE BOND STRENGTH OF A GLUED MANUFACTURER'S JOINT
Hardcopy , PDF
English
07-23-2013
1. Scope
2. Summary
3. Significance
4. Apparatus and materials
5. Test specimens
6. Conditioning
7. Procedure
8. Report
9. Internal bond strength of linerboard
10. Precision
11. Additional information
The bond strength of the glued manufacturer's joint of a corrugated box is measured in this method. Covers a maximum force applied at 90 degree to the plane of the joint, in a direction parallel to the length of the joint to propagate the failure of a segment of the corrugated box.
| DocumentType |
Provisional Test Method
|
| Pages |
4
|
| PublisherName |
Technical Association of the Pulp & Paper Industry
|
| Status |
Withdrawn
|
| TAPPI/ANSI T 402 sp:2013 | STANDARD CONDITIONING AND TESTING ATMOSPHERES FOR PAPER, BOARD, PULP HANDSHEETS, AND RELATED PRODUCTS |
| TAPPI T 541 : 2010 | INTERNAL BOND STRENGTH OF PAPERBOARD (Z-DIRECTION TENSILE) |