Standard Specification for Centrifugally Cast Ferritic/Austenitic Stainless Steel Pipe for Corrosive Environments
English
12-31-2010
11-11-2014
| Committee |
A 01
|
| DocumentType |
Standard
|
| Pages |
3
|
| ProductNote |
Reconfirmed 1997
|
| PublisherName |
American Society for Testing and Materials
|
| Status |
Superseded
|
| SupersededBy |
1.1 This specification covers centrifugally cast ferritic/ austenitic steel pipe intended for general corrosive service. These steels are susceptible to embrittlement if used for prolonged periods at elevated temperatures.
1.2 Optional supplementary requirements are provided when additional testing may be required.
1.3 The values stated in inch-pound units are to be regarded as the standard.