BS EN 438-8:2009
Withdrawn
View Superseded by
High-pressure decorative laminates (HPL). Sheets based on thermosetting resins (usually called laminates) Classification and specifications for design laminates
Hardcopy , PDF
English
04-30-2009
12-03-2018
Foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Material types and classification system
5 Requirements
5.1 Compliance
5.2 Inspection requirements
5.3 Dimensional tolerance requirements
5.4 Test requirements
Bibliography
Describes performance requirements for high-pressure decorative laminates (HPL) intended for interior use with a design effect surface having a phenolic based core and a decorative surface, not covered by EN 438-3 to EN 438-6.
| Committee |
PRI/52
|
| DevelopmentNote |
Supersedes 07/30172710 DC. (05/2009) Reviewed and confirmed by BSI, March 2014. (02/2014)
|
| DocumentType |
Standard
|
| Pages |
20
|
| PublisherName |
British Standards Institution
|
| Status |
Withdrawn
|
| SupersededBy | |
| Supersedes |
This part of EN 438 specifies performance requirements for high-pressure decorative laminates (HPL) intended for interior use with a design effect surface having a phenolic based core and a decorative surface, not covered by EN 438-3 to EN 438-6. Three surface material types (metal, wood veneer and pearlescent decor) are defined in this part of EN 438. EN 438-2 specifies the test methods relevant to this part of EN 438.
| Standards | Relationship |
| EN 438-8:2009 | Identical |
| DIN EN 438-8:2009-07 | Equivalent |
| I.S. EN 438-8:2009 | Equivalent |
| UNE-EN 438-8:2009 | Equivalent |
| ISO 4211-2:2013 | Furniture — Tests for surface finishes — Part 2: Assessment of resistance to wet heat |
| EN 12722:2009+A1:2013 | Furniture - Assessment of surface resistance to dry heat |
| ISO 11925-2:2010 | Reaction to fire tests — Ignitability of products subjected to direct impingement of flame — Part 2: Single-flame source test |
| EN 13823:2010+A1:2014 | Reaction to fire tests for building products - Building products excluding floorings exposed to the thermal attack by a single burning item |
| ISO 1183-1:2012 | Plastics — Methods for determining the density of non-cellular plastics — Part 1: Immersion method, liquid pyknometer method and titration method |
| EN 12721:2009+A1:2013 | Furniture - Assessment of surface resistance to wet heat |
| EN 438-2:2016 | High-pressure decorative laminates (HPL) - Sheets based on thermosetting resins (usually called laminates) - Part 2: Determination of properties |
| ISO 11664-2:2007 | Colorimetry — Part 2: CIE standard illuminants |
| ISO 4211-3:2013 | Furniture — Tests for surface finishes — Part 3: Assessment of resistance to dry heat |
| ISO 178:2010 | Plastics — Determination of flexural properties |
| EN ISO 1183-1:2012 | Plastics - Methods for determining the density of non-cellular plastics - Part 1: Immersion method, liquid pyknometer method and titration method (ISO 1183-1:2012) |