DEFSTAN 80-27/5(2009) : 2009
Withdrawn
PAINT, AMMUNITION FINISHING, BRUSHING, SPRAYING AND DIPPING TYPES: SEMI-GLOSS; MATT
English
01-01-2009
08-23-2018
Foreword
0 Introduction
1 Scope
2 Warning
3 Normative References
4 Description
5 Information to be Supplied by the Purchaser
6 Keeping Quality
7 Quality Assurance
8 Containers and Marking of Containers
9 Composition
10 Test Requirements
Annex A - Preparation of Painted Test Panels
Annex B - Resistance to White Spirit
Annex C - Resistance to Mineral Oil
Describes the requirements for an air-drying paint for finishing ammunition suitable for application to primed and/or pre-treated ferrous and non-ferrous substrates.
| DevelopmentNote |
Supersedes DEFSTAN 80-27/4(1998). (07/2009)
|
| DocumentType |
Standard
|
| Pages |
12
|
| PublisherName |
UK Ministry of Defence Standards
|
| Status |
Withdrawn
|
| Supersedes |
| SAE AMS03_11A | Phosphate Treatment of Iron and Steel |
| BS EN ISO 1514:2004 | Paints and varnishes. Standard panels for testing |
| DEFSTAN 80-207/2(2003) : 2003 | PAINT, PRIMING, ZINC CHROMATE, NON AIRCRAFT USE, LOW VOC SINGLE OR MULTI-PACK |
| DEFSTAN 03-11/5(2008) : 2008 | PHOSPHATE TREATMENT OF IRON AND STEEL |
| BS EN ISO 1518:2001 | Paints and varnishes. Scratch test |
| BS EN ISO 1513:1995 | Paints and varnishes. Examination and preparation of samples for testing |
| BS EN ISO 1517:1995 | Paints and varnishes. Surface-drying test. Ballotini method |
| DEFSTAN 80-126/1(1989) : 1989 | PAINT, PRIMING, ZINC PHOSPHATE, AIR-DRYING - TYPES: BRUSHING, SPRAYING, DIPPING |
| BS EN 23270:1991 | Specification for temperatures and humidities for conditioning and testing paints, varnishes and their raw materials |
| BS EN ISO 2431:2011 | Paints and varnishes. Determination of flow time by use of flow cups |
| DEFSTAN 91-39/3(2001) : 2001 | HYDRAULIC FLUID, PETROLEUM: ANTI-WEAR NATO CODE: H-576 JOINT SERVICE DESIGNATION: OM-33 |
| BS EN 29117:1992 | Methods of test for paints. Tests associated with paint film formation Paints and varnishes. Determination of through-dry state and through-dry time. Method of test |
| DEFSTAN 80-206/2(2003) : 2003 | PAINT, PRIMING, ZINC PHOSPHATE, NON AIRCRAFT USE, LOW VOC SINGLE OR MULTI-PACK |
| BS 245:1976 | Specification for mineral solvents (white spirit and related hydrocarbon solvents) for paints and other purposes |
| DEFSTAN 80-15/2(1990) : 1990 | PAINT, PRE-TREATMENT PRIMER (ETCHING PRIMER) - TYPES: BRUSHING (BASE AND ACID COMPONENT), SPRAYING (BASE AND ACID COMPONENT) |
| BS EN ISO 1519:2011 | Paints and varnishes. Bend test (cylindrical mandrel) |
| DEFSTAN 80-114/1(1985) : 1985 | PAINT, PRIMING, DEFENCE EQUIPMENT AIR DRYING - TYPES: BRUSHING, SPRAYING DIPPING |