ASTM A 599/A599M : 2007

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Standard Specification for Tin Mill Products, Electrolytic Tin-Coated, Cold-Rolled Sheet

Available format(s)

PDF

Language(s)

English

Published date

01-11-2007

Superseded date

11-11-2014

£50.78
Excluding VAT

CONTAINED IN VOL. 01.06, 2017 Defines cold-rolled steel sheet in coils or in cut lengths, tin-coated by electrodeposition.

Committee
A 01
DevelopmentNote
Supersedes ASTM A 599. (05/2002)
DocumentType
Standard
Pages
3
ProductNote
Reconfirmed 2007
PublisherName
American Society for Testing and Materials
Status
Superseded
SupersededBy
Supersedes

1.1 This specification covers cold-rolled steel sheet in coils or in cut lengths, tin-coated by electrodeposition. The product is commonly known as electrolytic tin-coated sheet, and is for applications that need good solderability, good surface appearance, and a degree of corrosion resistance. Tin-coated sheet is produced to various designations of tin coating, as outlined in Table 1.

1.1.1 Electrolytic tin-coated sheet is customarily available as commercial steel (CS); drawing steel (DS); deep drawing steel (DDS); extra deep drawing steel (EDDS), and structural steel (SS). The tin coating is available as unmelted or melted.

1.2 LimitationsThis specification is applicable to orders in either inch-pound units (as A 599), which is supplied in thicknesses from 0.015 in. to 0.036 in., or SI units [as A 599M], which is supplied in thicknesses from 0.381 mm to 0.914 mm. For thicknesses lighter than 0.015 in. [0.381 mm], refer to A 624 [A 624M].

1.3 Unless the order shows the M designation [SI units], the product shall be furnished to inch-pound units. The values stated in either inch-pound or SI units are to be regarded as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with this specification.

ASTM A 623M : 2016 : REDLINE Standard Specification for Tin Mill Products, General Requirements [Metric]
ASTM A 1008/A1008M : 2016-09 SPECIFICATION FOR STEEL, SHEET, COLD-ROLLED, CARBON, STRUCTURAL, HIGH-STRENGTH LOW-ALLOY, HIGH-STRENGTH LOW-ALLOY WITH IMPROVED FORMABILITY, SOLUTION HARDENED, AND BAKE HARDENABLE
ASTM A 623 : 2016 : REDLINE Standard Specification for Tin Mill Products, General Requirements
ASTM A 700 : 2014 Standard Guide for Packaging, Marking, and Loading Methods for Steel Products for Shipment

£50.78
Excluding VAT