BS HR 403:1973

Superseded

Superseded

A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.

View Superseded by

Specification for nickel-chromium-titanium heat-resisting alloy cold-worked and softened seamless tubes (nickel base, Cr 19.5, Ti 0.4)

Available format(s)

Hardcopy , PDF

Language(s)

English

Published date

30-03-1973

Superseded date

31-01-2011

Superseded by

BS 2HR 403:2011

£142.00
Excluding VAT

Describes the chemical composition mechanical properties and inspection and test requirements for nickel alloy seamless tubes.

Committee
ACE/61/-/48
DevelopmentNote
Supersedes 71/39034 DC. (06/2005) Reviewed and confirmed by BSI, December 2009. (11/2009)
DocumentType
Standard
Pages
6
PublisherName
British Standards Institution
Status
Superseded
SupersededBy

BS HR 203:1972 Specification for nickel-chromium-titanium heat-resisting alloy plate, sheet and strip (nickel base, Cr 19.5, Ti 0.4)
BS 2HR 504:1973 Specification for nickel-chromium-titanium heat-resisting alloy bar, wire and rivets (nickel base, Cr 19.5, Ti 0.4)
BS HR 5:1972 Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4)

BS HR 5:1972 Specification for nickel-chromium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 19.5, Ti 0.4)
BS 3763:1964 The International System of units (SI)
BS 2HR100(1971) : LATEST
BS HR 203:1972 Specification for nickel-chromium-titanium heat-resisting alloy plate, sheet and strip (nickel base, Cr 19.5, Ti 0.4)
BS 2HR 504:1973 Specification for nickel-chromium-titanium heat-resisting alloy bar, wire and rivets (nickel base, Cr 19.5, Ti 0.4)
BS 350:2004 Conversion factors for units

£142.00
Excluding VAT