PD CLC/TR 62662:2011

Current

Current

The latest, up-to-date edition.

Measurement procedures for materials used in photovoltaic modules Encapsulants. Test procedure of optical durability

Available format(s)

Hardcopy , PDF

Language(s)

English

Published date

31-12-2011

£232.00
Excluding VAT
Summarise this standard

FOREWORD
INTRODUCTION
1 Scope
2 Normative references
3 Terms and definitions
4 Description of brittle fracture
5 Identification of brittle fracture
6 Failure mechanisms
7 Risk assessment
8 Guidance for material selection and production
9 Preventive methods
Bibliography
Annex ZA (normative) - Normative references to
         international publications with their
         corresponding European publications

Gives an analysis of the risk of influencing factors for brittle fracture of composite insulators that are mostly loaded in the tensile mode (suspension and tension insulators).

Committee
PEL/36
DevelopmentNote
Renumbers and supersedes BS PD IEC/TR 62662. 2011 version incorporates corrigendum to BS PD IEC/TR 62662. (12/2011)
DocumentType
Standard
Pages
26
PublisherName
British Standards Institution
Status
Current
Supersedes

This technical report presents an analysis of the risk of influencing factors for brittle fracture of composite insulators that are mostly loaded in the tensile mode (suspension and tension insulators). Guidance is given to reduce the risk of in-service brittle fractures.

This phenomenon is limited to tension and suspension insulators. However, the general information given concerning the importance of various parameters can be used as a guideline for the design and production of any kind of composite insulator.

Standards Relationship
CLC/TR 62662:2011 Identical

£232.00