SN EN 13235 : 2006
Current
The latest, up-to-date edition.
ADVANCED TECHNICAL CERAMICS - MECHANICAL PROPERTIES OF CERAMIC COMPOSITES AT HIGH TEMPERATURE UNDER INERT ATMOSPHERE - DETERMINATION OF CREEP BEHAVIOUR
12-01-2013
Foreword
1 Scope
2 Normative references
3 Principle
4 Terms, definitions and symbols
5 Significance and use
6 Apparatus
6.1 Test installations
6.2 Load train
6.3 Test chamber
6.4 Set-up for heating
6.5 Extensometer
6.6 Temperature measurement
6.7 Data recording system
6.8 Micrometers
7 Test specimens
8 Test specimen preparation
8.1 Machining and preparation
8.2 Number of test specimens
9 Test procedures
9.1 Test set-up: temperature considerations
9.2 Test set-up: loading considerations
9.3 Test set-up: measurement of test specimen dimensions
9.4 Test technique
9.5 Test validity
10 Calculation of results
10.1 Test specimen origin
10.2 Results
10.3 Creep strain rate curve
11 Test report
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.