TAPPI T 234 : 0

Current

Current

The latest, up-to-date edition.

COARSENESS OF PULP FIBERS

Available format(s)

Hardcopy , PDF

Language(s)

English

1. Scope and summary
2. Apparatus
3. Materials
4. Preparations of specimen slide
5. Procedure
6. Calculation
7. Report
8. Additional information
Literature cited

Measures the coarseness (weight per unit length) of the fibers in a pulp by counting the crossings of a known weight of fibers per unit area on a prepared slide over lines of known length. The crossings are counted with a microscope and mechanical stage, by traversing the slide over a series of 5-cm distances.

DocumentType
Classical Method
Pages
6
PublisherName
Technical Association of the Pulp & Paper Industry
Status
Current

TAPPI UM 258 : 2010 LABORATORY PROCESSING OF PULP (KOLLERGANG METHOD)
ASTM D 7357 : 2007 Standard Specification for Cellulose Fibers for Fiber-Reinforced Concrete
TAPPI T 232 : 2013 FIBER LENGTH OF PULP BY PROJECTION
ASTM D 7357 : 2007 : R2012 Standard Specification for Cellulose Fibers for Fiber-Reinforced Concrete

View more information
£41.84
Excluding VAT

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.