BS EN ISO 3672-2:2001
Current
The latest, up-to-date edition.
Plastics. Unsaturated-polyester resins (UP-R) Preparation of test specimens and determination of properties
Hardcopy , PDF
English
14-05-2002
Foreword
Introduction
1 Scope
2 Normative references
3 Preparation of test specimens
3.1 General
3.2 Pretreatment of materials
3.3 Preparation of the sheets
3.4 Cutting out test specimens
4 Conditioning of test specimens
5 Determination of properties
Gives the methods of preparation of test specimens and test methods used for the determination of the properties of unsaturated-polyester resins. Also gives the requirements for handling test material and for conditioning both the test material before moulding and the specimens before testing. The properties of crosslinked unsaturated-polyester resins have been selected from the general test methods in ISO 10350-1. Other test methods in wide use for, or of particular significance to, unsaturated-polyester resins (particularly properties useful for the processing of non-crosslinked resins) are also included in this part of ISO 3672.
Committee |
PRI/42
|
DevelopmentNote |
Renumbers and supersedes BS ISO 3672-2 Supersedes 96/121473 DC. (11/2001) 2001 Version incorporates amendment 13326 to BS ISO 3672-2. (10/2005)
|
DocumentType |
Standard
|
Pages |
22
|
PublisherName |
British Standards Institution
|
Status |
Current
|
Supersedes |
Standards | Relationship |
SN EN ISO 3672-2 : 2001 | Identical |
NEN EN ISO 3672-2 : 2001 | Identical |
UNI EN ISO 3672-2 : 2003 | Identical |
I.S. EN ISO 3672-2:2002 | Identical |
ISO 3672-2:2000 | Identical |
NBN EN ISO 3672-2 : 2001 | Identical |
EN ISO 3672-2 : 2001 | Identical |
NF EN ISO 3672-2 : 2002 | Identical |
UNE-EN ISO 3672-2:2002 | Identical |
NS EN ISO 3672-2 : 1ED 2001 | Identical |
DIN EN ISO 3672-2:2002-07 | Identical |
DIN EN ISO 3672-2 E : 2002 | Identical |
IEC 60243-1:2013 | Electric strength of insulating materials - Test methods - Part 1: Tests at power frequencies |
IEC 60695-11-20:2015 | Fire hazard testing - Part 11-20: Test flames - 500 W flame test method |
IEC 60112:2003+AMD1:2009 CSV | Method for the determination of the proof and the comparative tracking indices of solid insulating materials |
ISO 2719:2016 | Determination of flash point — Pensky-Martens closed cup method |
ISO 6603-2:2000 | Plastics — Determination of puncture impact behaviour of rigid plastics — Part 2: Instrumented impact testing |
ISO 2535:2001 | Plastics Unsaturated-polyester resins Measurement of gel time at ambient temperature |
EN ISO 62:2008 | Plastics - Determination of water absorption (ISO 62:2008) |
ISO 2114:2000 | Plastics (polyester resins) and paints and varnishes (binders) Determination of partial acid value and total acid value |
ISO 3521:1997 | Plastics — Unsaturated polyester and epoxy resins — Determination of overall volume shrinkage |
EN ISO 8256:2004 | Plastics - Determination of tensile-impact strength (ISO 8256:2004) |
ISO 3167:2014 | Plastics Multipurpose test specimens |
EN ISO 2114:2000/AC:2005 | PLASTICS (POLYESTER RESINS) AND PAINTS AND VARNISHES (BINDERS) - DETERMINATION OF PARTIAL ACID VALUE AND TOTAL ACID VALUE |
IEC 60250:1969 | Recommended methods for the determination of the permittivity and dielectric dissipation factor of electrical insulating materials at power, audio and radio frequencies including metre wavelengths |
ISO 3219:1993 | Plastics — Polymers/resins in the liquid state or as emulsions or dispersions — Determination of viscosity using a rotational viscometer with defined shear rate |
ISO 14848:1998 | Plastics — Unsaturated-polyester resins — Determination of reactivity at 130 degrees C |
EN 59:2016 | Glass reinforced plastics - Determination of indentation hardness by means of a Barcol hardness tester |
EN ISO 527-2:2012 | Plastics - Determination of tensile properties - Part 2: Test conditions for moulding and extrusion plastics (ISO 527-2:2012) |
ISO 6271:2015 | Clear liquids Estimation of colour by the platinum-cobalt colour scale |
ISO 10350-1:2017 | Plastics — Acquisition and presentation of comparable single-point data — Part 1: Moulding materials |
EN ISO 178:2010/A1:2013 | PLASTICS - DETERMINATION OF FLEXURAL PROPERTIES (ISO 178:2010/AMD 1:2013) |
ISO 8256:2004 | Plastics — Determination of tensile-impact strength |
EN ISO 1675:1998 | Plastics - Liquid resins - Determination of density by the pyknometer method (ISO 1675:1985) |
EN ISO 604 : 2003 | PLASTICS - DETERMINATION OF COMPRESSIVE PROPERTIES (ISO 604:2002) |
ISO 11359-2:1999 | Plastics Thermomechanical analysis (TMA) Part 2: Determination of coefficient of linear thermal expansion and glass transition temperature |
ISO 3672-1:2000 | Plastics Unsaturated-polyester resins (UP-R) Part 1: Designation system |
EN ISO 2818:1996 | PLASTICS - PREPARATION OF TEST SPECIMENS BY MACHINING |
EN ISO 527-1:2012 | Plastics - Determination of tensile properties - Part 1: General principles (ISO 527-1:2012) |
EN ISO 179-1:2010 | Plastics - Determination of Charpy impact properties - Part 1: Non-instrumented impact test (ISO 179-1:2010) |
ISO 75-2:2013 | Plastics — Determination of temperature of deflection under load — Part 2: Plastics and ebonite |
ISO 527-2:2012 | Plastics — Determination of tensile properties — Part 2: Test conditions for moulding and extrusion plastics |
ISO 11357-2:2013 | Plastics Differential scanning calorimetry (DSC) Part 2: Determination of glass transition temperature and glass transition step height |
ISO 1523:2002 | Determination of flash point — Closed cup equilibrium method |
EN ISO 75-2:2013 | Plastics - Determination of temperature of deflection under load - Part 2: Plastics and ebonite (ISO 75-2:2013) |
ISO 4615:1979 | Plastics Unsaturated polyesters and epoxide resins Determination of total chlorine content |
IEC 60296:2012 RLV | Fluids for electrotechnical applications - Unused mineral insulating oils for transformers and switchgear |
EN ISO 3167:2014 | Plastics - Multipurpose test specimens (ISO 3167:2014) |
EN ISO 3521 : 1999 | Plastics - Unsaturated polyester and epoxy resins - Determination of overall volume shrinkage (ISO 3521:1997) |
ISO 4630:2015 | Clear liquids Estimation of colour by the Gardner colour scale |
IEC 60093:1980 | Methods of test for volume resistivity and surface resistivity of solid electrical insulating materials |
ISO 2554:1997 | Plastics — Unsaturated polyester resins — Determination of hydroxyl value |
ISO 2577:2007 | Plastics Thermosetting moulding materials Determination of shrinkage |
ISO 1675:1985 | Plastics — Liquid resins — Determination of density by the pyknometer method |
IEC 60695-11-10:2013 | Fire hazard testing - Part 11-10: Test flames - 50 W horizontal and vertical flame test methods |
EN ISO 3219:1994 | Plastics - Polymers/resins in the liquid state or as emulsions or dispersions - Determination of viscosity using a rotational viscometer with defined shear rate (ISO 3219:1993) |
ISO 291:2008 | Plastics Standard atmospheres for conditioning and testing |
EN ISO 6603-2:2000 | Plastics - Determination of puncture impact behaviour of rigid plastics - Part 2: Instrumented puncture test (ISO 6603-2:2000) |
ISO 604:2002 | Plastics — Determination of compressive properties |
ISO 179-1:2010 | Plastics — Determination of Charpy impact properties — Part 1: Non-instrumented impact test |
EN ISO 4589-2:2017 | Plastics - Determination of burning behaviour by oxygen index - Part 2: Ambient-temperature test (ISO 4589-2:2017) |
ISO 62:2008 | Plastics Determination of water absorption |
EN ISO 291:2008 | Plastics - Standard atmospheres for conditioning and testing (ISO 291:2008) |
EN ISO 2554 : 1999 | PLASTICS - UNSATURATED POLYESTER RESINS - DETERMINATION OF HYSROXYL VALUE |
EN 22719 : 1993 | PETROLEUM PRODUCTS AND LUBRICANTS - DETERMINATION OF FLASH POINT - PENSKY-MARTENS CLOSED CUP METHOD |
ISO 4589-2:2017 | Plastics — Determination of burning behaviour by oxygen index — Part 2: Ambient-temperature test |
ISO 2818:1994 | Plastics — Preparation of test specimens by machining |
ISO 4901:2011 | Reinforced plastics based on unsaturated-polyester resins Determination of the residual styrene monomer content, as well as the content of other volatile aromatic hydrocarbons, by gas chromatography |
ISO 760:1978 | Determination of water Karl Fischer method (General method) |
EN ISO 4615 : 1999 | Plastics - Unsaturated polyesters and epoxide resins - Determination of total chlorine content (ISO 4615:1979) |
ISO 178:2010 | Plastics Determination of flexural properties |
EN ISO 2535 : 2002 | PLASTICS - UNSATURATED POLYESTER RESINS - MEASUREMENT OF GEL TIME AT AMBIENT TEMPERATURE (ISO 2535:2001) |
ISO 527-1:2012 | Plastics Determination of tensile properties Part 1: General principles |
Please Login or Create an Account so you can add users to your Multi user PDF Later.
Important note : All end users must be registered with an Account prior to user licenses being assigned.
Users cannot be edited or removed once added to your Multi user PDF.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.